Consumption
1.8~2 kg/mm/m² Note: This figure is theoretical and does not include for any additional material required due to surface porosity, surface profile, variations in level and wastage etc.
Application instructions
Mixing
▪ Chanye-epomota 6500A and Chanye-epomota 6500B mixed at weight ratio of 1:1.
▪ Mix with a high-speed drill (> 650 rpm) and an egg beater style mixing paddle to blend for approximately 1~2 minutes, until to minimize entrapped air and uniform mix has been produced.
▪ Pour 3.7~4 kg of clean, cool potable water into the mixing container, ensuring strict control of the water content (do not over-water).
▪ Add 25 kg Chanye-epomota 6500C to the mixing container, while slowly mixing, adding the complete contents of the bag.
▪ Mix with a high-speed drill (> 650 rpm) and an egg beater style mixing paddle to blend resin and powder for approximately 2~3 minutes, until a lump-free and uniform mix has been produced.
Note: Operating time: 10 ~ 15 minutes (temperature: + 15 ° C(+59°F) ~ + 35 ° C(+95°F))
Application
▪ Pour the mix and spread evenly, and control the material thickness by scrape rake.
▪ Even surfaces by smoothing trowel.
▪ Roll immediately with a spiked roller to ensure even thickness and achieve defoaming effect.