Поделиться:
Item:2.5Y25000 | Result | Technical Requirement | Test Method |
Tow Denier | 25000 | ±900 | YC/T 26–2008 |
Variation Coefficiency, Total Denier | ≤0.21 | ≤0.6 | YC/T 26–2008 |
Denier per Filament | 2.5 | ±0.22 | YC/T 26–2008 |
Crimp Number/25mm | 24 | ±4 | YC/T 26–2008 |
Breaking Strength N/Ktex | 21.6 | ≥18 | YC/T 26–2008 |
Section Shape | Y | YC/T 26–2008 | |
Moisture % | 5.2 | 6.0±1.6 | YC/T 26–2008 |
Oil Content % | 1.1 | 0.7-1.5 | YC/T 26–2008 |
Acetone Residual% | 0.07 | ≤0.3 | YC/T 26–2008 |
Titanium Dioxide Content% | 0.39 | 0.4±0.2 | YC/T 26–2008 |
Item:2.5Y30000 | Result | Technical Requirement | Test Method |
Tow Denier | 30000 | ±900 | YC/T 26–2008 |
Variation Coefficiency, Total Denier | ≤0.21 | ≤0.6 | YC/T 26–2008 |
Denier per Filament | 2.5 | ±0.22 | YC/T 26–2008 |
Crimp Number/25mm | 24 | ±4 | YC/T 26–2008 |
Breaking Strength N/Ktex | 21.6 | ≥18 | YC/T 26–2008 |
Section Shape | Y | YC/T 26–2008 | |
Moisture % | 5.2 | 6.0±1.6 | YC/T 26–2008 |
Oil Content % | 1.1 | 0.7-1.5 | YC/T 26–2008 |
Acetone Residual% | 0.07 | ≤0.3 | YC/T 26–2008 |
Titanium Dioxide Content% | 0.39 | 0.4±0.2 | YC/T 26–2008 |